Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Dow Corning Z-6137 SILANE

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer Dow Corning
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning Z-6137 SILANE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Aminofunctional silane homopolymer adhesion promoterInformation provided by Dow Corning
Physical Properties Metric English Comments
Volatiles 76 %
76 %
Kinematic Viscosity 6.75 cSt
6.75 cSt
Thermal Properties Metric English Comments
Flash Point 100 °C
212 °F
closed cup
Optical Properties Metric English Comments
Refractive Index 1.40
1.40
Processing Properties Metric English Comments
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Active Content (%) 22