Dow Corning Z-6076 SILANE

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer Dow Corning
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning Z-6076 SILANE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3-chloropropyltrimethoxysilaneInformation provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 1.09 g/cc

@Temperature 25.0 °C
1.09 g/cc

@Temperature 77.0 °F
Molecular Weight 198.5 g/mol
198.5 g/mol
Thermal Properties Metric English Comments
Boiling Point 196 °C
385 °F
Flash Point 51.0 °C
124 °F
closed cup
Optical Properties Metric English Comments
Refractive Index 1.418
1.418
Processing Properties Metric English Comments
Shelf Life 36.0 Month
36.0 Month
Descriptive Properties Value Comments
Appearance clear liquid
Color light yellow
Purity (%) 97