Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Dow Corning Z-6010 CHLOROSILANE

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer Dow Corning
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning Z-6010 CHLOROSILANE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3-chloropropyltrichlorosilane clc3h6sicl3 - intermediate in synthesis of organoreactive silanes.Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 1.35 g/cc
1.35 g/cc
Thermal Properties Metric English Comments
Boiling Point 182.8 °C
361.0 °F
Flash Point 84.0 °C
183 °F
closed cup
Descriptive Properties Value Comments
Active Content (%) 100
Users viewing this material also viewed the following: