Material Notes:
Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 1.23 g/cc
1.23 g/cc
Kinematic Viscosity 4.2 cSt
4.2 cSt
Molecular Weight 253.2 g/mol
253.2 g/mol
Thermal Properties Metric English Comments
Boiling Point 35.0 °C
95.0 °F
Flash Point 93.0 °C
199 °F
closed cup
Processing Properties Metric English Comments
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Appearance colorless
Copyright © lookpolymers.com All Rights Reserved