Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Dow Corning Z-1219 DIMETHYLDICHLOROSILANE

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer Dow Corning
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning Z-1219 DIMETHYLDICHLOROSILANE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Dimethyldichlorosilane (ch3)2sicl2 - synthesis of silanes, silicones; hydrophobic treatment; pyrolysis to si-c coatings; protective group in organic synthesis.Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 1.07 g/cc
1.07 g/cc
Kinematic Viscosity 0.44 cSt
0.44 cSt
Vapor Pressure 0.1531 bar

@Temperature 25.0 °C
114.8 torr

@Temperature 77.0 °F
Thermal Properties Metric English Comments
Melting Point -74.0 °C
-101 °F
Boiling Point 70.0 °C
158 °F
Flash Point -3.80 °C
25.2 °F
closed cup
Processing Properties Metric English Comments
Shelf Life 60.0 Month
60.0 Month
Descriptive Properties Value Comments
Appearance colorless
Copyright © lookpolymers.com All Rights Reserved