Dow Corning Y-30 ANTIFOAM EMULSION

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer Dow Corning
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning Y-30 ANTIFOAM EMULSION.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Dow Corning Antifoam Y-30 Emulsion is a water-dilutable, 30 percent active silicone emulsion designed to control foam in aqueous systems.Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 1.00 g/cc

@Temperature 25.0 °C
1.00 g/cc

@Temperature 77.0 °F
pH 3.0
3.0
Viscosity 2500 cP
2500 cP
dynamic
Processing Properties Metric English Comments
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Active Content (%) 30
Color white
Non-Ionic yes