Dow Corning XIAMETER® PMCPPMX-200 50CS Silicone Fluid

Category Fluid
Manufacturer Dow Corning
Trade Name XIAMETER®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning XIAMETER® PMCPPMX-200 50CS Silicone Fluid.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Is chemically equivalent to DOW CORNING® 200 FLUID 50CS. 100% active, 50 cSt, polydimethylsiloxane polymer.Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 0.960 g/cc

@Temperature 25.0 °C
0.960 g/cc

@Temperature 77.0 °F
Viscosity Measure 50 cSt
50 cSt
Kinetic/Kinematic
Surface Tension 20.8 dynes/cm
20.8 dynes/cm
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 200 °C
392 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Pour Point -70.0 °C
-94.0 °F
Flash Point >= 100 °C
>= 212 °F
Closed Cup
>= 285 °C
>= 545 °F
Open Cup
Optical Properties Metric English Comments
Refractive Index 1.401
1.401
Descriptive Properties Value Comments
Hydrophobic Yes