Dow Corning XIAMETER® PMCPOHX-4010 Polymer 4000CS

Category Polymer , Thermoset , Silicone
Manufacturer Dow Corning
Trade Name XIAMETER®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning XIAMETER® PMCPOHX-4010 Polymer 4000CS.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Is chemically equivalent to DOW CORNING® 3-0213 POLYMER, 4000CS. Polydimethylsiloxane polymer with terminated, curable silanol functionality, viscosity = 4,000 cp.Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 0.975 g/cc

@Temperature 25.0 °C
0.975 g/cc

@Temperature 77.0 °F
Viscosity 3500 - 4500 cP
3500 - 4500 cP
Dynamic
Processing Properties Metric English Comments
Shelf Life 60.0 Month
60.0 Month
Descriptive Properties Value Comments
Silanol Content (%) 0.126
Users viewing this material also viewed the following: