Dow Corning SZ-1328E Silicone Surfactant

Category Fluid , Polymer , Thermoset , Silicone
Manufacturer Dow Corning
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning SZ-1328E Silicone Surfactant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Dow Corning® SZ-1328E Additive is a non-hydrolyzable silicone surfactant recommended for production of high-resiliency molded PU foam.Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 0.970 g/cc

@Temperature 25.0 °C
0.970 g/cc

@Temperature 77.0 °F
Thermal Properties Metric English Comments
Flash Point 161 °C
322 °F
open cup
Descriptive Properties Value Comments
Appearance colorless
Color pale yellow