Dow Corning SYLGARD® PMCP309 Silicone Surfactant

Category Fluid , Polymer , Thermoset , Silicone
Manufacturer Dow Corning
Trade Name SYLGARD®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning SYLGARD® PMCP309 Silicone Surfactant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Low molecular weight nonionic silicone polyether surfactant, developed to improve the wetting, spreading, and penetration of agricultural chemicals.Information provided by Dow Corning
Physical Properties Metric English Comments
Solids Content 100 %
100 %
Viscosity Measure 40 cSt
40 cSt
Kinetic/Kinematic
Thermal Properties Metric English Comments
Flash Point >= 100 °C
>= 212 °F
Closed cup
Processing Properties Metric English Comments
Shelf Life 36.0 Month
36.0 Month
Descriptive Properties Value Comments
Active Content (%) 100
Cloud Point (°C) 3
Color Amber Clear
HLB Ratio (%) 12
Non-Ionic Yes