Dow Corning SYL-OFF® SL 70 RELEASE MODIFIER

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer Dow Corning
Trade Name SYL-OFF®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning SYL-OFF® SL 70 RELEASE MODIFIER.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Solvent-free, fast curing, efficient release modification at all peel speeds, excellent bath stabilitym, formulated without catalystInformation provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 1.04 g/cc
1.04 g/cc
Viscosity 1000 cP
1000 cP
dynamic
Processing Properties Metric English Comments
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Active Content (%) 100
Appearance clear liquid
Solvent solventless