Dow Corning SYL-OFF® SL 3000 CATALYST

Category Other Engineering Material , Catalyst/Initiator , Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Dow Corning
Trade Name SYL-OFF®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning SYL-OFF® SL 3000 CATALYST.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
1,000 ppm platinum in vinyl polymerInformation provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 0.960 g/cc
0.960 g/cc
Viscosity 300 cP
300 cP
dynamic
Processing Properties Metric English Comments
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Appearance clear liquid
Solvent solventless