Material Notes:
Syl-Off® EM 7974 is an emulsion based silicone release coating, excellent for bakery release performance and is specifically developed for application during the paper making process.Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 0.990 g/cc

@Temperature 25.0 °C
0.990 g/cc

@Temperature 77.0 °F
pH 5.0
5.0
Thermal Properties Metric English Comments
Flash Point >= 100 °C
>= 212 °F
Closed cup
Processing Properties Metric English Comments
Shelf Life 9.00 Month
9.00 Month
Descriptive Properties Value Comments
Active Content (%) 40
Color Milky White
Water Resistant Yes