Dow Corning SYL-OFF® PMCP7923 Catalyst Emulsion

Category Other Engineering Material , Catalyst/Initiator
Manufacturer Dow Corning
Trade Name SYL-OFF®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning SYL-OFF® PMCP7923 Catalyst Emulsion.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Syl-Off® 7923 Catalyst Emulsion is a 40% solids emulsion of vinyl functional polymer and platinum catalyst in water. A high performance catalyst recommended where fast cure speed is required.Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 0.990 g/cc

@Temperature 25.0 °C
0.990 g/cc

@Temperature 77.0 °F
pH 5.0
5.0
Thermal Properties Metric English Comments
Flash Point >= 100 °C
>= 212 °F
Closed cup
Processing Properties Metric English Comments
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Active Content (%) 40
Color Milky White