Dow Corning SYL-OFF® PMCP7041 Modifier

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer Dow Corning
Trade Name SYL-OFF®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning SYL-OFF® PMCP7041 Modifier.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Syl-Off® 7041 Release Modifier is a 100% active solids release modifier compatible with hexenyl functional polymers. Offers paricularly stable release and fast cure. Recommeded for use with Syl-Off® 7040 Coating.Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 1.04 g/cc

@Temperature 25.0 °C
1.04 g/cc

@Temperature 77.0 °F
Viscosity Measure 2000 cSt
2000 cSt
Kinetic/Kinematic
Thermal Properties Metric English Comments
Flash Point <= 100 °C
<= 212 °F
Closed cup
Processing Properties Metric English Comments
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Active Content (%) 100
Color Colorless Pale Yellow