Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Dow Corning SLYGARD® Q3-3600 A&B THERMALLY CONDUCTIVE ENCAPSULANT

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone , Silicone Rubber , Silicone, RTV, Encapsulation Grade
Manufacturer Dow Corning
Trade Name SLYGARD®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning SLYGARD® Q3-3600 A&B THERMALLY CONDUCTIVE ENCAPSULANT.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Two-part, grey, 1:1, heat cure, excellent flow, self-priming, thermally conductive, low viscosity.Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 2.13 g/cc
2.13 g/cc
Viscosity 4700 cP
4700 cP
dynamic
Mechanical Properties Metric English Comments
Hardness, Shore A 87
87
Tensile Strength, Ultimate 6.60 MPa
957 psi
Elongation at Break 55 %
55 %
Thermal Properties Metric English Comments
Thermal Conductivity 0.770 W/m-K
5.34 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 200 °C
392 °F
Minimum Service Temperature, Air -45.0 °C
-49.0 °F
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
Dielectric Strength 26.0 kV/mm
660 kV/in
Processing Properties Metric English Comments
Cure Time 30.0 min

@Temperature 150 °C
0.500 hour

@Temperature 302 °F
heat cure
60.0 min

@Temperature 100 °C
1.00 hour

@Temperature 212 °F
heat cure
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Color grey
Flowable yes
Hydrophobic yes
Mix Ratio (X:1) 100
Base to Catalyst
Self Leveling yes
Water Resistant yes
Working Time (min) 1440