Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Dow Corning SILASTIC® S-2 RTV SILICONE RUBBER BASE & CURING AGENT

Category Polymer , Adhesive , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone , Silicone Rubber , Silicone, RTV, Adhesive/Sealant Grade
Manufacturer Dow Corning
Trade Name SILASTIC®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning SILASTIC® S-2 RTV SILICONE RUBBER BASE & CURING AGENT.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High strength, lower durometer silicone rubber suited for many moldmaking applications. Silastic S-2 is recommended for use with plaster, cement and rigid polyurethane and can be used with polyesters.Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 1.13 g/cc

@Temperature 25.0 °C
1.13 g/cc

@Temperature 77.0 °F
Viscosity 9000 cP
9000 cP
mixing, dynamic
Mechanical Properties Metric English Comments
Hardness, Shore A 20
20
Tensile Strength, Ultimate 6.27 MPa
910 psi
Elongation at Break 600 %
600 %
Tear Strength 22.8 kN/m
130 pli
Descriptive Properties Value Comments
Color off-white
Mix Ratio (X:1) 10
Base to Catalyst
Working Time (min) 60
Copyright © lookpolymers.com All Rights Reserved