Dow Corning SILASTIC® M-3 RTV SILICONE RUBBER BASE & CURING AGENT

Category Polymer , Adhesive , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone , Silicone Rubber , Silicone, RTV, Adhesive/Sealant Grade
Manufacturer Dow Corning
Trade Name SILASTIC®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning SILASTIC® M-3 RTV SILICONE RUBBER BASE & CURING AGENT.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Dow Corning Silastic® M-3 RTV Silicone Rubber is an addition cured (platinum catalyzed); high durometer silicone rubber developed for use in prototyping, architectural, and furniture applications where dimensional tolerances and fast cure rate at room temperature are critical.Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 1.29 g/cc

@Temperature 25.0 °C
1.29 g/cc

@Temperature 77.0 °F
Viscosity 70000 cP
70000 cP
dynamic
Mechanical Properties Metric English Comments
Hardness, Shore A 62
62
Tensile Strength, Ultimate 4.48 MPa
650 psi
Elongation at Break 240 %
240 %
Tear Strength 14.0 kN/m
80.0 pli
Descriptive Properties Value Comments
Color blue
Mix Ratio (X:1) 10
Base to Catalyst
Working Time (min) 20