Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Dow Corning SILASTIC® LS 5-8720 FLUOROSILICONE RUBBER

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone , Silicone Rubber
Manufacturer Dow Corning
Trade Name SILASTIC®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning SILASTIC® LS 5-8720 FLUOROSILICONE RUBBER.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
20 Durometer, off-white, Fluorosilicone Base.Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 1.30 g/cc

@Temperature 25.0 °C
1.30 g/cc

@Temperature 77.0 °F
Mechanical Properties Metric English Comments
Hardness, Shore A 20
20
Tensile Strength, Ultimate 8.48 MPa
1230 psi
Elongation at Break 699 %
699 %
Tear Strength 3.94 kN/m
22.5 pli
Processing Properties Metric English Comments
Shelf Life 36.0 Month
36.0 Month
Descriptive Properties Value Comments
Color off-white