Dow Corning SILASTIC® FL 40-9201 A&B KIT

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone , Silicone Rubber
Manufacturer Dow Corning
Trade Name SILASTIC®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning SILASTIC® FL 40-9201 A&B KIT.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
40 shore A 100% fluorinated liquid silicone rubber. Designed for effective manufacturing of automotive parts that must wistand harsh environment, such as fuel contact under extreme temperatures.Information provided by Dow Corning
Mechanical Properties Metric English Comments
Hardness, Shore A 35 - 45
35 - 45
Tensile Strength, Ultimate 8.27 MPa
1200 psi
Elongation at Break 300 %
300 %
Tear Strength 17.5 kN/m
100 pli
Descriptive Properties Value Comments
Appearance translucent
part B
Color straw yellow
part A
Mix Ratio (X:1) 100
Base to Catalyst ETN