Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Dow Corning SILASTIC® 9416/20E KIT PARTS A&B

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone , Silicone Rubber
Manufacturer Dow Corning
Trade Name SILASTIC®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning SILASTIC® 9416/20E KIT PARTS A&B.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
30 Durometer, 2-part, 1 to 1 mix, opaque, Auto connector seal grade, Liquid Silicone Rubber.Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 1.11 g/cc

@Temperature 25.0 °C
1.11 g/cc

@Temperature 77.0 °F
Mechanical Properties Metric English Comments
Hardness, Shore A 16
16
Tensile Strength, Ultimate 4.5001 MPa
652.68 psi
Elongation at Break 995 %
995 %
Tear Strength 11.01 kN/m
62.83 pli
Compression Set 20 %
20 %
Processing Properties Metric English Comments
Pot Life 4320 min
4320 min
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Appearance opaque
Mix Ratio (X:1) 100
Base to Catalyst ETN