Dow Corning SILASTIC® 94-595-HC SILICONE RUBBER PART A&B

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone , Silicone Rubber
Manufacturer Dow Corning
Trade Name SILASTIC®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning SILASTIC® 94-595-HC SILICONE RUBBER PART A&B.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
30 Durometer, 2-part, 1 to 1 mix, translucent, Injection Moulding grade, Liquid Silicone Rubber.Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 1.12 g/cc

@Temperature 25.0 °C
1.12 g/cc

@Temperature 77.0 °F
Solids Content 100 %
100 %
Mechanical Properties Metric English Comments
Hardness, Shore A 42
42
Tensile Strength, Ultimate 10.1 MPa
1460 psi
Tensile Strength, Yield 1.03 MPa
150 psi
at 150% elongation, maximum
Elongation at Break 610 %
610 %
Tear Strength 33.3 kN/m
190 pli
Compression Set 47 %
47 %
Processing Properties Metric English Comments
Pot Life 1440 min
1440 min
Shelf Life 18.0 Month
18.0 Month
Descriptive Properties Value Comments
Appearance translucent
Mix Ratio (X:1) 100
Base to Catalyst ETN