Dow Corning SILASTIC® 9280/70E KIT PARTS A&B

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone , Silicone Rubber
Manufacturer Dow Corning
Trade Name SILASTIC®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning SILASTIC® 9280/70E KIT PARTS A&B.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
70 Durometer, 2 parts, 1 to 1 mix, translucent, injection molding grade Liquide Silicone Rubber.Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 1.15 g/cc

@Temperature 25.0 °C
1.15 g/cc

@Temperature 77.0 °F
Solids Content 100 %
100 %
Viscosity 560000 cP
560000 cP
Mechanical Properties Metric English Comments
Hardness, Shore A 68
68
Tensile Strength, Ultimate 8.3999 MPa
1218.3 psi
Elongation at Break 360 %
360 %
Tear Strength 44.05 kN/m
251.3 pli
Compression Set 49 %
49 %
Electrical Properties Metric English Comments
Volume Resistivity 9.00e+15 ohm-cm
9.00e+15 ohm-cm
Processing Properties Metric English Comments
Pot Life 4320 min
4320 min
Shelf Life 15.0 Month
15.0 Month
Descriptive Properties Value Comments
Appearance translucent
Mix Ratio (X:1) 100
Base to Catalyst ETN