Dow Corning SILASTIC® 9220/55 KIT PARTS A&B

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone , Silicone Rubber
Manufacturer Dow Corning
Trade Name SILASTIC®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning SILASTIC® 9220/55 KIT PARTS A&B.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
55 Durometer, 2-part, 1 to 1 mix, black Liquid Silicone Rubber.Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 1.28 g/cc

@Temperature 25.0 °C
1.28 g/cc

@Temperature 77.0 °F
Solids Content 100 %
100 %
Mechanical Properties Metric English Comments
Hardness, Shore A 53
53
Tensile Strength, Ultimate 8.00 MPa
1160 psi
Elongation at Break 530 %
530 %
Tear Strength 35.1 kN/m
200 pli
Compression Set 20 %
20 %
Electrical Properties Metric English Comments
Volume Resistivity 2.00e+15 ohm-cm
2.00e+15 ohm-cm
Dielectric Strength 1.14 kV/mm
29.0 kV/in
Processing Properties Metric English Comments
Pot Life 4320 min
4320 min
Shelf Life 15.0 Month
15.0 Month
Descriptive Properties Value Comments
Color black
Mix Ratio (X:1) 100
Base to Catalyst ETN