Material Notes:
80 Durometer, peroxide cured, low compression set Silicone Rubber CompoundInformation provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 1.39 g/cc

@Temperature 25.0 °C
1.39 g/cc

@Temperature 77.0 °F
Mechanical Properties Metric English Comments
Hardness, Shore A 79
79
Tensile Strength, Ultimate 7.460 MPa
1082 psi
Tensile Strength, Yield 5.38 MPa
781 psi
at 100% elongation, maximum
Elongation at Break 108 %
108 %
Tear Strength 11.6 kN/m
66.0 pli
Descriptive Properties Value Comments
Color red