Dow Corning SILASTIC® 1604-T SILICONE RUBBER

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone , Silicone Rubber
Manufacturer Dow Corning
Trade Name SILASTIC®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning SILASTIC® 1604-T SILICONE RUBBER.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
65 Durometer, peroxide cured, cable grade Silicone Rubber Compounds used for electrical/general cable and appliance wire. It has high mechanical properties, and color options and customization options are available.Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 1.23 g/cc

@Temperature 25.0 °C
1.23 g/cc

@Temperature 77.0 °F
Mechanical Properties Metric English Comments
Hardness, Shore A 66
66
Tensile Strength, Ultimate 9.729 MPa
1411 psi
Tensile Strength, Yield 2.22 MPa
322 psi
at 100% elongation, maximum
Elongation at Break 443 %
443 %
Processing Properties Metric English Comments
Shelf Life 6.00 Month
6.00 Month