Material Notes:
OH end-blocked polydimethylsiloxane, visc. 55-90 cst., OH/Silanol content 1.0-1.7%.Information provided by Dow Corning
Processing Properties Metric English Comments
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Active Content (%) 100
Silanol Content (%) 1-1.7