Dow Corning OS-2 SILICONE CLEANER & SURFACE PREP

Category Fluid
Manufacturer Dow Corning
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning OS-2 SILICONE CLEANER & SURFACE PREP.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Non Ozone depleting, VOC exempt, Silicone cleaner to clean Plastic and Metals, excellent for removing oils, silicone-based car wax and protectants.Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 0.780 g/cc

@Temperature 25.0 °C
0.780 g/cc

@Temperature 77.0 °F
Volatile Organic Compounds (VOC) Content 0.00 g/l
0.00 g/l
Viscosity Measure 0.78 cSt
0.78 cSt
kinetic/kinematic
Vapor Pressure 0.04212 bar

@Temperature 25.0 °C
31.59 torr

@Temperature 77.0 °F
Thermal Properties Metric English Comments
Melting Point -80.0 °C
-112 °F
Boiling Point 109 °C
228 °F
Flash Point -3.00 °C
26.6 °F
closed cup
Processing Properties Metric English Comments
Shelf Life 24.0 Month
24.0 Month