Material Notes:
Rolling element bearing grease for high speed applicationInformation provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 0.910 g/cc

@Temperature 25.0 °C
0.910 g/cc

@Temperature 77.0 °F
Mechanical Properties Metric English Comments
Four Ball Extreme Pressure, Weld Load 203.9 kg
449.6 lb (mass)
Penetration P(60), 1/10 mm 280
280
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 150 °C
302 °F
Minimum Service Temperature, Air -20.0 °C
-4.00 °F
Dropping Point >= 260 °C
>= 500 °F
Descriptive Properties Value Comments
Color yellowish-brown
NLGI Number 2
Thickening System lithium complex