Dow Corning MG 7-9850 SOFT SKIN ADHESIVE KIT (A&B)

Category Polymer , Adhesive , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone , Silicone Rubber
Manufacturer Dow Corning
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning MG 7-9850 SOFT SKIN ADHESIVE KIT (A&B).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Two-part, platinum-catalyzed, fillerless, elastomeric silicone adhesive. This clear and soft skin adhesive is intended for wound care applications, including over-the-counter bandages and scar therapies.Information provided by Dow Corning
Physical Properties Metric English Comments
Viscosity 2800 cP
2800 cP
dynamic
Mechanical Properties Metric English Comments
Penetration P(60), 1/10 mm 135
135
Processing Properties Metric English Comments
Pot Life 30 min
30 min