Dow Corning HV 1660/65 LIGHT GRAY SILICONE RUBBER KP

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone , Silicone Rubber
Manufacturer Dow Corning
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning HV 1660/65 LIGHT GRAY SILICONE RUBBER KP.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
65 Shore hardness high consistency silicone rubber with excellent tracking and erosion resistance, excellent wet electrial properties,high voltage insulation applications.Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 1.56 g/cc

@Temperature 25.0 °C
1.56 g/cc

@Temperature 77.0 °F
Mechanical Properties Metric English Comments
Hardness, Shore A 65
65
Tensile Strength, Ultimate 4.21 MPa
610 psi
Elongation at Break 280 %
280 %
Tear Strength 13.1 kN/m
75.0 pli
Electrical Properties Metric English Comments
Volume Resistivity 2.00e+14 ohm-cm
2.00e+14 ohm-cm
Dielectric Constant 3.67

@Frequency 100 Hz
3.67

@Frequency 100 Hz
Dielectric Strength 17.4 kV/mm
441 kV/in
Dissipation Factor 0.017

@Frequency 100 Hz
0.017

@Frequency 100 Hz
Processing Properties Metric English Comments
Shelf Life 6.00 Month
6.00 Month
Descriptive Properties Value Comments
Color grey
Hydrophobic yes
Water Resistant yes