Material Notes:
40 Shore Hardness Conductive liquid silicone rubber with high tear strength, high electrical conductivity and fast cure speedInformation provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 1.07 g/cc

@Temperature 25.0 °C
1.07 g/cc

@Temperature 77.0 °F
Solids Content 100 %
100 %
Mechanical Properties Metric English Comments
Hardness, Shore A 40
40
Tensile Strength, Ultimate 6.00 MPa
870 psi
Elongation at Break 400 %
400 %
Tear Strength 29.8 kN/m
170 pli
Electrical Properties Metric English Comments
Volume Resistivity 17 ohm-cm
17 ohm-cm
Processing Properties Metric English Comments
Pot Life 4320 min
4320 min
Shelf Life 6.00 Month
6.00 Month
Descriptive Properties Value Comments
Color black
Mix Ratio (X:1) 100
Base to Catalyst ETN