Dow Corning DM5 Demulsifier

Category Polymer , Thermoset , Silicone
Manufacturer Dow Corning
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning DM5 Demulsifier.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Silicone polyether, acts as a performance booster for crude oil emulsion breakers.Information provided by Dow Corning
Physical Properties Metric English Comments
Viscosity Measure 350 cSt
350 cSt
Kinetic/Kinematic
Thermal Properties Metric English Comments
Flash Point >= 60.0 °C
>= 140 °F
Closed cup
Descriptive Properties Value Comments
HLB Ratio (%) 10