Material Notes:
Two-part, clear, 1:1, addition cure, low temperature cure, low viscosity, controlled volatility.Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 0.980 g/cc

@Temperature 25.0 °C
0.980 g/cc

@Temperature 77.0 °F
Viscosity 100 cP
100 cP
dynamic
Mechanical Properties Metric English Comments
Hardness, Shore OO 70
70
Penetration P(60), 1/10 mm 75
75
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 150 °C
302 °F
Minimum Service Temperature, Air -45.0 °C
-49.0 °F
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
Dielectric Constant 2.5

@Frequency 1.00e+6 Hz
2.5

@Frequency 1.00e+6 Hz
Dielectric Strength 14.0 kV/mm
356 kV/in
Dissipation Factor <= 0.00010

@Frequency 100 Hz
<= 0.00010

@Frequency 100 Hz
<= 0.00010

@Frequency 100000 Hz
<= 0.00010

@Frequency 100000 Hz
Processing Properties Metric English Comments
Cure Time 30.0 min

@Temperature 70.0 °C
0.500 hour

@Temperature 158 °F
Shelf Life 18.0 Month
18.0 Month
Descriptive Properties Value Comments
Appearance clear
Flowable yes
Hydrophobic yes
Self Leveling yes
Water Resistant yes
Working Time (min) 120