Dow Corning BF 20 PLUS ANTIFOAM EMULSION

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer Dow Corning
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning BF 20 PLUS ANTIFOAM EMULSION.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
20% active silicone antifoam emulsion suitable for controlling foam in end-use applications of many liquid detergent products.Information provided by Dow Corning
Physical Properties Metric English Comments
Volatiles 73 - 77 %
73 - 77 %
pH 3.5 - 5.0
3.5 - 5.0
Viscosity 700 cP
700 cP
dynamic
Processing Properties Metric English Comments
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Active Content (%) 20
Non-Ionic yes