Dow Corning ANTIFOAM C EMULSION, MEDICAL

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer Dow Corning
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning ANTIFOAM C EMULSION, MEDICAL.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Water-dilutable emulsion containing 30% simethicone USP by weight and methylcelluloseInformation provided by Dow Corning
Physical Properties Metric English Comments
pH 2.5
2.5
Descriptive Properties Value Comments
Siloxane Content (%) 29.4