Material Notes:
Conventional acetoxy RTV sealant with adhesion promoterInformation provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 1.03 g/cc
1.03 g/cc
Mechanical Properties Metric English Comments
Hardness, Shore A 25
25
Tensile Strength, Ultimate 2.31 MPa
335 psi
Elongation at Break 500 %
500 %
Processing Properties Metric English Comments
Cure Time 1440 min

@Temperature 22.0 °C
24.0 hour

@Temperature 71.6 °F
Shelf Life 30.0 Month
30.0 Month
Descriptive Properties Value Comments
Appearance clear
Color Aluminum
Black
White
Water Resistant yes