Dow Corning 7-3101 Elastomer Blend Hip Emulsion

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer Dow Corning
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning 7-3101 Elastomer Blend Hip Emulsion.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A concentrated emulsion of dimethicone crosspolymer in cyclopentasiloxane and dimethicone that is designed to facilitate the rapid development of skin care formulations which contain these emollients. Typical applications include: suncare, body lotions, body washes, wipes, and color cosmetics.Information provided by Dow Corning
Physical Properties Metric English Comments
Solids Content 15 %
15 %
Viscosity 30000 cP
30000 cP
Dynamic