Dow Corning 5-8601 FLUOROSILICONE LSR, KIT

Category Polymer , Thermoset , Silicone
Manufacturer Dow Corning
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning 5-8601 FLUOROSILICONE LSR, KIT.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Fluorosilicone rubber designed for liquid injection moldingInformation provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 1.30 g/cc

@Temperature 25.0 °C
1.30 g/cc

@Temperature 77.0 °F
Mechanical Properties Metric English Comments
Hardness, Shore A 45
45
Tensile Strength, Ultimate 6.21 MPa
900 psi
Elongation at Break 350 %
350 %
Tear Strength 19.3 kN/m
110 pli
Electrical Properties Metric English Comments
Dielectric Strength 15.7 kV/mm
400 kV/in
Arc Resistance 200 sec
200 sec
Processing Properties Metric English Comments
Pot Life 5760 min
5760 min
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Appearance transparent
Color red