Material Notes:
DOW CORNING 5-7113 Silicone Quat Microemulsion is a 22% non-ionic emulsion of cationized amino-functional silicone polymer. This emulsion was developed as a conditioning additive for hair care products such as shampoos, conditioners and styling aids. The product provides easy formulation and dilution stability.Information provided by Dow Corning
Physical Properties Metric English Comments
pH 6.0 - 8.0
6.0 - 8.0
Kinematic Viscosity 10 cSt
10 cSt
Descriptive Properties Value Comments
Active Content (%) 25
Appearance translucent
Non-Ionic yes