Material Notes:
Non-ionic, 35% active, emulsion of a medium viscosity trimethylsilyl terminated polydimethylsiloxane. This product has been replaced by Dow Corning® IE 39 EmulsionInformation provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 0.990 g/cc

@Temperature 25.0 °C
0.990 g/cc

@Temperature 77.0 °F
pH 6.5 - 8.5
6.5 - 8.5
Processing Properties Metric English Comments
Shelf Life 15.0 Month
15.0 Month
Descriptive Properties Value Comments
Active Content (%) 35-85
Color milky white
Non-Ionic yes
Users viewing this material also viewed the following: