Dow Corning 3559 NEUTRAL ADHESIVE SEALANT BLACK

Category Polymer , Adhesive , Thermoset , Silicone , Silicone, RTV, Adhesive/Sealant Grade
Manufacturer Dow Corning
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning 3559 NEUTRAL ADHESIVE SEALANT BLACK.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DOW CORNING 3559 is a black, 1- component, non-flowing, silicone adhesive with fast deep section cure. It forms high strength, medium modulus flexible bonds to metal, glass, ceramic substrates and many engineering plastics with improved adhesion properties when exposed to high temperatures. It withstands temperatures up to 220°C.Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 1.30 g/cc
1.30 g/cc
Mechanical Properties Metric English Comments
Elongation at Break 400 %
400 %
Processing Properties Metric English Comments
Shelf Life 9.00 Month
9.00 Month
Descriptive Properties Value Comments
Color black