Dow Corning 3110 BASE & 4 CATALYST

Category Polymer , Thermoset , Silicone
Manufacturer Dow Corning
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning 3110 BASE & 4 CATALYST.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
General purpose low viscosity silicone mold making rubber suited for the reproduction of objects with no deep undercuts or complex shapes. 3110 Base with 4 Catalyst is recommended for use with rigid polyurethane and can be used with plaster, wax and polyurathanes.Information provided by Dow Corning
Descriptive Properties Value Comments
Approximate De-mold Time (hours) 0.33
Mix Ratio (X:1) 200
Base to Catalyst ETN
Working Time (min) 5