Dow Corning 3-6752 THERMALLY CONDUCTIVE ADHESIVE

Category Polymer , Adhesive , Thermoset , Silicone , Silicone, RTV, Adhesive/Sealant Grade
Manufacturer Dow Corning
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning 3-6752 THERMALLY CONDUCTIVE ADHESIVE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
One-part, grey, rapid heat cure and primerless adhesion to common substrates used in the electronics industry.Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 2.60 g/cc

@Temperature 25.0 °C
2.60 g/cc

@Temperature 77.0 °F
Viscosity 81000 cP
81000 cP
dynamic
Mechanical Properties Metric English Comments
Hardness, Shore A 87
87
Tensile Strength, Ultimate 3.76 MPa
545 psi
Elongation at Break 15 %
15 %
Thermal Properties Metric English Comments
Thermal Conductivity 1.80 W/m-K
12.5 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 200 °C
392 °F
Minimum Service Temperature, Air -45.0 °C
-49.0 °F
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Volume Resistivity 7.10e+13 ohm-cm
7.10e+13 ohm-cm
Dielectric Constant 5.5

@Frequency 100000 Hz
5.5

@Frequency 100000 Hz
5.6

@Frequency 100 Hz
5.6

@Frequency 100 Hz
Dielectric Strength 15.7 kV/mm
400 kV/in
Dissipation Factor <= 0.00010

@Frequency 100000 Hz
<= 0.00010

@Frequency 100000 Hz
0.0070

@Frequency 100 Hz
0.0070

@Frequency 100 Hz
Processing Properties Metric English Comments
Cure Time 3.00 min

@Temperature 150 °C
0.0500 hour

@Temperature 302 °F
10.0 min

@Temperature 125 °C
0.167 hour

@Temperature 257 °F
40.0 min

@Temperature 100 °C
0.667 hour

@Temperature 212 °F
Shelf Life 6.00 Month
6.00 Month
Descriptive Properties Value Comments
Color grey
Flowable yes
Hydrophobic yes
Self Leveling yes
Water Resistant yes