Material Notes:
Two-part, translucent green, firm, fast RT or heat cure, and primerless chemical adhesion.Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 0.970 - 0.980 g/cc

@Temperature 25.0 °C
0.970 - 0.980 g/cc

@Temperature 77.0 °F
Viscosity 340 cP
340 cP
dynamic
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 150 °C
302 °F
Minimum Service Temperature, Air -45.0 °C
-49.0 °F
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
Dielectric Constant 2.64

@Frequency 100 Hz
2.64

@Frequency 100 Hz
2.64

@Frequency 100000 Hz
2.64

@Frequency 100000 Hz
Dielectric Strength 13.8 kV/mm
350 kV/in
Dissipation Factor 0.00020

@Frequency 100000 Hz
0.00020

@Frequency 100000 Hz
<= 0.0010

@Frequency 100 Hz
<= 0.0010

@Frequency 100 Hz
Processing Properties Metric English Comments
Cure Time 1.00 min

@Temperature 150 °C
0.0167 hour

@Temperature 302 °F
1.50 min

@Temperature 125 °C
0.0250 hour

@Temperature 257 °F
2.00 min

@Temperature 100 °C
0.0333 hour

@Temperature 212 °F
1.20 - 60.0 min

@Temperature 22.0 °C
0.0200 - 1.00 hour

@Temperature 71.6 °F
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Appearance translucent
Color green
Flowable yes
Gel Hardness (Grams/Penetration) 270
Hydrophobic yes
Self Leveling yes
Water Resistant yes
Working Time (min) <5
Users viewing this material also viewed the following: