Material Notes:
A water-dispersible dimethicone copolyol wax for use in skincare, woundcare, haircare, suncare, and antiperspirants and deodorant applications.Information provided by Dow Corning
Thermal Properties Metric English Comments
Flash Point >= 100 °C
>= 212 °F
Closed cup