Dow Corning 170 CATALYST

Category Other Engineering Material , Catalyst/Initiator
Manufacturer Dow Corning
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning 170 CATALYST.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Liquid. Slow cure. 50% dispersion of an organotin complex in perchloroethylene.Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 1.005 g/cc

@Temperature 25.0 °C
1.005 g/cc

@Temperature 77.0 °F
Solids Content 50 %
50 %
Thermal Properties Metric English Comments
Flash Point >= 100 °C
>= 212 °F
closed cup
Descriptive Properties Value Comments
Appearance clear liquid
Color pale straw
Solvent Perchloroethylene
Users viewing this material also viewed the following: