Dow Corning 1204 RTV PRIME COAT

Category Polymer , Thermoset , Silicone
Manufacturer Dow Corning
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning 1204 RTV PRIME COAT.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Clear primer in naphtha solvent for use with all one-part alcohol cure and two-part condensation cure silicone elastomersInformation provided by Dow Corning
Physical Properties Metric English Comments
Volatile Organic Compounds (VOC) Content 774 g/l
774 g/l
Thermal Properties Metric English Comments
Flash Point 8.00 °C
46.4 °F
closed cup
Processing Properties Metric English Comments
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Appearance clear
Hydrophobic yes
Solvent VM&P Naphtha
Water Resistant yes