Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Dow C758-80NA Polypropylene Impact Copolymer Resin

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer , Polypropylene, Impact Modified; Molded/Extruded
Manufacturer Dow Chemical
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow C758-80NA Polypropylene Impact Copolymer Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
OverviewVery easy mold filling and fast set upGood balance of impact strength and stiffnessContains a nucleating and antistatic additiveComplies with: U.S. FDA FCN 843, Canadian HPFB No ObjectionDOW C758-80NA Polypropylene Resin is a nucleated, antistatic, very high flow, reactor grade polypropylene impact copolymer. It provides excellent processability, while maintaining a good balance of impact and stiffness. DOW C758-80NA Polypropylene Resin is intended for use injection molded automotive interior trim applications.Dow Announced Sale of Global Polypropylene Business to Braskem in July 2011.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D792
Melt Index of Compound 80 g/10 min

@Load 2.16 kg,
Temperature 230 °C
80 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 25.7 MPa
3730 psi
ASTM D638
Elongation at Yield 4.6 %
4.6 %
ASTM D638
Flexural Modulus, 1% Secant 1380 MPa
200000 psi
ASTM D790A
Izod Impact, Notched 0.747 J/cm
1.40 ft-lb/in
ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 106 °C
223 °F
Unannealed; ASTM D648