Material Notes:
Dow Polypropylene Impact Copolymer Resins are semi-crystalline thermoplastic materials that can provide a combination of desirable properties and affordability: low density; excellent chemical resistance and ESCR; excellent moisture barrier; good gloss; good impact over wide range of temperature and low water absorption. Dow Polypropylene Impact Copolymer resins are suitable for a wide range of applications and may be fabricated by injection molding, blow molding and extrusion. C700-35N Polypropylene Impact Copolymer resin is a nucleated product suitable for injection molding.Data provided by Dow Chemical.Dow Announced Sale of Global Polypropylene Business to Braskem in July 2011.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM Data
Melt Flow 35 g/10 min

@Load 2.16 kg,
Temperature 230 °C
35 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM Data
Mechanical Properties Metric English Comments
Tensile Strength, Yield 27.6 MPa
4000 psi
ASTM Data
Izod Impact, Notched 0.694 J/cm
1.30 ft-lb/in
ASTM Data
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 115 °C
239 °F
Unannealed; ASTM Data